MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions PlenStar™ JAP61A Vinyl Compound - Wire & Cable  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes:

Description/Features:

  • UL Recognized Plenum Cable Compound per UL QMTM2
  • UL 60°C
  • Security and Fire Alarm
  • Low Smoke
  • Flame Retardant
  • Meets UL 13 requirements
  • CL2P
  • CL3P
  • Meets UL 1424 requirements
  • FPLP
  • Meets UL 444 Flame requirements
  • CMP
  • CAT-1

Applications:

  • Plenum Rated Telecommunication Jacket

Market:

  • Wire & Cable

Processing Method:

  • Extrusion Coating
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.
Hopper drying of compound pellets is recommended.

Information provided by PolyOne Corporation.

Geon® Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.59 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 9015 sec; ASTM D2240
Hardness, Shore D 4815 sec; ASTM D2240
Tensile Strength, Yield 2509 psiType 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break 259 %Type 4 - Flexibles, 20 in/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature 26.6 °FASTM D746
Oxygen Index 38.6 %0.075 in; ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 340 - 370 °FExtrusion
 
Descriptive Properties
Product FormPellets/Cubes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Wire & Cable JJC32A Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJJC32L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJJC310L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJJC330 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJJC309L PVC, Flexible

PH1PO3026 / 44853

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.