MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a paste consistency epoxy adhesive designed for bonding metals and many high temperature plastics such as fiberglass reinforced plastic, polyester, and phonetics

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 60 - 200 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 85
Tensile Strength, Ultimate 10000 psi
Elongation at Break <= 2.0 %
Modulus of Elasticity 750 ksi
Shear Strength 400 psi
@Temperature 177 °C
Aluminum Overlap
 600 psi
@Temperature 149 °C
Aluminum Overlap
 1500 psi
@Temperature 121 °C
Aluminum Overlap
 3000 psi
@Temperature -53.0 °C
Aluminum Overlap
 4500 psi
@Temperature 24.0 °C
Aluminum Overlap
 4500 psi
@Temperature 82.0 °C
Aluminum Overlap
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.80e+13 ohm-cm
Surface Resistance 9.80e+12 ohm
Dielectric Constant 10.5
@Temperature 23.0 °C
ASTM D150
 11.1
@Temperature 60.0 °C
ASTM D150
 16.7
@Temperature 90.0 °C
ASTM D150
 24
@Temperature 104 °C
ASTM D150
Dielectric Strength 77.0 kV/in
@Thickness 0.930 mm
Dissipation Factor 0.126
@Temperature 23.0 °C
 0.346
@Temperature 90.0 °C
 0.463
@Temperature 60.0 °C
 0.515
@Temperature 104 °C
Arc Resistance 76 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 49.0 µm/m-°C
@Temperature 0.000 - 80.0 °C
Thermal Conductivity 2.77 BTU-in/hr-ft²-°F
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2214 Regular Gray One-Part Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
3M Scotch-Weld™ DP460 NS Epoxy Adhesive

PMM34630 / 169377

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.