MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical C5 Product
Categories: Fluid

Material Notes: Structure & Characteristics: Obtained as a by-product from pyrolysis oil hydration plant which was produced from naphtha pyrolysis process, and C5 content is higher than 95%. Although it is in liquid phase in room temperature and pressure, it easily vaporizes in room temperature.

Uses: Used to blend gasoline

CAS: 78-78-4, 109-66-0 and 287-92-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.630 g/cc
Volatiles 100 %
@Temperature 21.0 °C
Vapor Pressure 426 torr
@Temperature 20.0 °C
Vapor Density=2.5
 
Thermal PropertiesOriginal ValueComments
Melting Point -130 °C
Boiling Point 36.0 °C
Flash Point -49.0 °C
Ignition Temperature 260 °CAutoignition
 
Descriptive Properties
Components1-Pentane2.1%
 2,2-Dimethy-butane4.4%
 2-Methy-1 — butene5.6%
 2-methy-2-butene17.7%
 BENZENE<1%
 C4<5%
 C5 PURITY>95%
 C6’s0.02%
 cis-2-Pentene3.8%
 cyclo-Pentane4.1%
 cyclo-Pentene10.6%
 iso-Pentane14.2%
 n-Pentane22.3%
 Other0.0108
 trans-2-Pentene14.1%
 T-SULFUR<300 ppm
Cu Corrosion<1
Gum Existent<2 mg/100ml
Oxidation>480 min
RVP<18 PSIG37.8°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Texatherm®
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Solvay Chemicals SOLKANE® 143a
ExxonMobil 603 Mobiltherm 600 Series
Evonik Polyoil 130 Polybutadiene

PLAY762 / 148772

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.