MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Zircar Ceramics SALI Alumina Insulation
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.480 g/cc
Open Porosity 84 %
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 2.07 MPaParallel to thickness
Compressive Yield Strength 1.31 MPaat 10% Compression, Parallel to thickness
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
@Temperature 20.0 - 1100 °C
Specific Heat Capacity 0.250 BTU/lb-°F
Thermal Conductivity 0.200 W/m-K
@Temperature 400 °C
Parallel to Thickness; ASTM C177-76
 0.310 W/m-K
@Temperature 800 °C
Parallel to Thickness; ASTM C177-76
 0.390 W/m-K
@Temperature 1400 °C
Parallel to Thickness; ASTM C177-76
Melting Point 1870 °C
Maximum Service Temperature, Air 1700 °C
Softening Point 1100 °CTemperature sample yields under load of push rod in CTE determination
Shrinkage 2.0 %SAG/Distortion, 6in. (152mm) x 1in. (25.4mm) x 1in. (25.4mm), 5in. (127mm) Span, % after 24 hrs. at 1650°C
 1.0 %
@Temperature 1650 °C,
Time 86400 sec
Perpendicular to Thickness
 3.0 %
@Temperature 1700 °C,
Time 86400 sec
Perpendicular to Thickness
 
Component Elements PropertiesOriginal ValueComments
Al2O3 80 %
SiO2 20 %
 
Descriptive Properties
BondSilica
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Ceramics AL-25/1700 Alumina Insulation
Zircar Ceramics AL-30 Alumina Insulation
Zircar Ceramics AL-30AA Alumina Insulation
Zircar Ceramics AL-30AAH Alumina Insulation
Zircar Ceramics ECO-20AA Alumina Insulation

CZIR043 / 2851

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.