MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Special Metals Nickel 222  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Pure Element

Material Notes: Wrought nickel with an addition of magnesium for electronic applications. The magnesium provides activation for cathodes of thermionic devices. Used for sleeves of indirectly heated oxide-coated cathodes. Ferromagnetic. Standard product forms are strip, tube, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: ASTM F 239; BS 3504; DIN 17740; Werkstoff Nr. 2.4053, Nickel, Ni
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.89 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 100Estimated from Vickers.
Hardness, Rockwell B 54Estimated from Vickers.
Hardness, Vickers 100Annealed
Tensile Strength, Ultimate 380 MPaAnnealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000880 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.3 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 75.0 W/m-K
Melting Point 1435 - 1446 °C
Solidus 1435 °C
Liquidus 1446 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu <= 0.10 %
Iron, Fe <= 0.10 %
Magnesium, Mg 0.010 - 0.10 %
Manganese, Mn <= 0.30 %
Nickel, Ni >= 99 %Including Cobalt
Silicon, Si <= 0.10 %
Sulfur, S <= 0.0080 %
Titanium, Ti <= 0.0050 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals Nickel 200
Special Metals Nickel 201
California Fine Wire Nickel 211 (Nickel Manganese Alloy)
Special Metals Nickel 205
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel

NINC04 / 17391

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.