MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC F-Clean® Film for Greenhouses
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: F-CLEAN®, produced by Asahi Glass Company, Ltd., is a Ethylene-Tetrafluoroethylene copolymer (ETFE) film used as the preferred covering material for horticultural greenhouses.
  • High tensile strength compared with other plastic films
  • High visible light transmission exceeds 90% and provides an environment inside the greenhouse very similar to outdoors.
  • Low degradation from sunlight and heat. Useful lifetime usually exceeds ten years.
  • Very easily cleaned by rain and snow.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.75 g/ccASTM D792
Water Absorption 0.030 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 39.0 MPaJIS K7127
Elongation at Break 200 - 510 %JIS K7127
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 2.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 120 kV/mmASTM D149
Dissipation Factor 0.00060
@Frequency 60 Hz
ASTM D150
 0.00080
@Frequency 1000 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
ASTM D150
 0.010
@Frequency 1e+9 Hz
ASTM D150
Arc Resistance 120 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 94.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point 260 °C
Maximum Service Temperature, Air 150 - 180 °CContinuous
 
Descriptive Properties
Chemical ResistanceExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC F-Clean® GRUV
AGC Fluon® FC 103 PTFE, 15% Glass Filled
Afton Plastics HT2183 Ethylene Tetrafluoroethylene
Bamberger Polymers Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade
BASF Ecoflex® F BX 7011 Biodegradable Plastic

PAGC85 / 23044

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.