MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain Versilon ™ Silver Antimicrobial Tubing
Categories: Polymer; Thermoplastic

Material Notes: Formerly Tygon® S3™ Silver Antimicrobial Tubing.
  • Plasticizer-free inner bore
  • Formulated with a silver based compound on I.D. surface
  • O.D. surface can also be formulated with a silver based compound
  • Reduces formulation of biofilm and mildew
  • Inhibits growth of microbes
  • Will not discolor
  • Meets FDA and NSF 51criteria
  • Contains no chemicals listed in California's Prop 65
  • Contains no BPA or phthalates

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Water Absorption <= 0.010 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 69
@Time 15.0 sec
ASTM D2240
Tensile Strength 2300 psiASTM D412
Tensile Stress at Strain 990 psi
@Strain 100 %
Elongation at Break 350 %ASTM D412
Tear Strength 250 pliASTM D1004
Compression Set 63 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395 Method B
Tensile Set 63 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °F
Brittleness Temperature -31.0 °FASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA Yes
NSF Yes
 
Descriptive Properties
ColorTranslucent Silver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® S3™ B-44-3 Bio-based Beverage Tubing Formulation
Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation
Saint-Gobain Norton® Tygon® R-3603 Laboratory and Vacuum Tubing Formulation
Process Technologies Inc BUNA-N Sanitary Gasket
Overview of materials for Thermoset Fluoroelastomer

PSTGQ901 / 160397

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.