Notes: Monprene RG-29068 NAT is specifically designed for regulated applications including food contact and is suitable for extrusion. Monprene RG-29068 NAT complies with various US FDA and European regulations and directives for food contact. Availability: Africa & Middle East; Europe; Latin America; North America Features: Food Contact Acceptable; Good Organoleptic Properties; Low Density; Medium Hardness Uses: Consumer Applications; Food Containers; Food Packaging RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion Preliminary data. Information provided by Teknor Apex |