MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® UH 2606 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Aliphatic, anionic polyurethane dispersion containing polycarbonate; solvent-free. Binder for the formulation of water-reducible coatings for plastic substrates and wood materials.

Properties / Applications: The product was designed specifically for the coating of plastic substrates. In addition the use in the formulation of PVC floor coatings, the binder exhibits a high grade property profile on a variety of substrates. Filler and topcoat applications (one and two-component) are also plausible. Other possibilities are wood and furniture applications. Bayhydrol UH 2606 yields coatings with good leveling, chemical and weather stabilities. They are also characterized by a tough but flexible property profile. Very good combinations are possible with polyester, polyurethane and acrylic dispersions. These must be checked on a case-by-case basis. Combinations with waterborne UV systems are also possible. Resistances can also be improved by post-curing with e.g. Bayhydur®. The mixing ratio of mill base to hardener is generally 10 : 1. Bayhydrol UH 2606 requires coalescing agents for film formation. Good results have been achieved with mixtures of butyl glycol/butyl diglycol/Dowanol TPnB (0.6 : 0.6 : 3.8).

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 64 - 66 %1g/1h/125°C; DIN EN ISO 3251
Particle Size 100 µm
pH 7.0 - 9.0DIN ISO 976

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fainplast Compounds GS 7016 Flexible PVC, Injection Molding for Footwear
Inovyn 250SB Polyvinyl Chloride General Purpose - Rigid
Geon® Performance Solutions Vinyl Cellular E2500 PVC, Rigid
Karina 805-18/105-IS-SD Gray PVC Compound
Geon® Performance Solutions 1250-xx01D Vinyl Compound - Wire & Cable

PCOVEST0178 / 201961

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.