Weather resistant grade. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Features: Good mold release, low viscosity, weather resistant , Uses: general purposes, automobile applications, LEDs Automotive Specifications: GM GMP.PC.009, Appearance: clear, transparent, Forms: pellets, Processing Method: Injection moldingInformation provided by Teijin Chemicals Ltd. |