Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product profile: - High strength, high burst pressure in tube form
- To 62% based on renewable raw material
- Good chemical resistance
- High strength
- Ductile, resilient in conditioned stage
- Moderate water absorption
- Low density
Grilamid 2S 20 natural is suitable for applications at moderate continuous use temperature and without repeated direct exposure to UV radiation. Preferred applications:- Injection molded functional parts
- Bushes, gears
- Consumer goods
- Semi-fabricates such as tubes, film, sheet, profiles
- Sheathing and guides
Information provided by EMS Grivory.
|