MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Corr-Paint™ CP4055 High Temperature Protective Silicone Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: Chrome oxide green, electrical insulation coating for use on power resistors for applications to 1100°F (593°C).

Vendors: Aremco offers a broad range of coatings formulated using an advanced water-based silicone emulsion combined with inorganic fillers and pigments to offer VOC compliant coatings. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/cc
Solids Content 38.1 %38.1 %Volume
 55 %55 %Weight
Volatiles 5.9 %5.9 %
Viscosity 500 - 1000 cP500 - 1000 cP
Thickness 1.00 microns0.0394 milDry Film Thickness
 2.60 microns0.102 milWet Film Thickness
Storage Temperature 12.8 - 29.4 °C55.0 - 85.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 593 °C1100 °F
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 48.9 °C50.0 - 120 °FApplication Temperature
Dry Time >= 1.00 hour>= 1.00 hourCuring, Min Air Set
 1.00 - 2.00 hour1.00 - 2.00 hourTouch
 2.00 - 4.00 hour2.00 - 4.00 hourHandling
 1.00 - 24.0 hour1.00 - 24.0 hourRecoat
Cure Time  45.0 min
@Temperature 249 °C
0.750 hour
@Temperature 480 °F
Option B
 60.0 min
@Temperature 232 °C
1.00 hour
@Temperature 450 °F
Option A
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorPale Green
Theoretical Dry Film Coverage, ft2/gal612
ThinnerDistilled Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAREM972 / 316317

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.