Hostalen ACP 6031D is a high density polyethylene resin used in small blow molding applications such as thin-wall packaging and consumer goods. It exhibits very high stiffness. Hostalen ACP 6031D is delivered in pellet form, contains antioxidants and has a broad molecular weight distribution. Hostalen ACP 6031D is not intended for use in medical and pharmaceutical applications. Applications: Bottles For Consumer Goods, Bottles for Industrial Use, Jerry Cans, Sports, Leisure & ToysInformation provided by LyondellBasell. |