MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Devcon® Flexane® High Performance Putty Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: A tough, rubber-like urethane compound for making a broad range of repairs to protect against wear, abrasion, and noise reduction. Uses: Protect equipment surfaces from wear and abrasion. Protect processing equipment such as coating hoppers, lining chutes, pump volutes, impellers, and fan housings. Features: Excellent tear resistance, Mixes easily, Bonds (with primers) to metal, concrete, rubber, wood, and fiberglass, Highly resistant to impact and abrasion, Trowels on smoothly.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0426 lb/in³Cured
Solids Content 88 %By volume
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78ASTM D2240
Tensile Strength 4500 psiUrethanes; ASTM D412
Elongation at Break <= 600 %ASTM D412
Tear Strength 400 pliASTM D624
Taber Abrasion, mg/1000 Cycles 0.119Cured 7 days at 75°F. 1000g, 1000 revs. H-18, dry
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 13.8 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °FWet
 180 °FDry
Shrinkage 12 %Linear During cure; ASTM D2566
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hour
@Temperature 24.0 °C
Functional cure
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 10.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Chemical/Solvent Resistance1,1,1-Trichloroethane: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Aluminum Sulfate 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting Oil: Fair30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Isopropyl Alcohol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric 50%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric Acid 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Potassium Hydroxide 40%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric 50%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Xylene: poor30 day immersion at 75°F. Sample cured 7 days at RT
ColorBlackCured
Coverage94 in.²/lbCured. @ 1/4"
Demolding Time10 hrs
Mix Ratio by weight94 to 6Resin/Hardener
Specific Volume (in.³/lb)23.5Cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9185 / 239695

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.