MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the melt strength ideally suited for blow molding and other applications requiring ultra high melt viscosity. It exhibits improved strength, stiffness and creep resistance compare to standard blow molding grades. Outstanding permeability and chemical resistance to oils, hydrocarbons and most solvents are other advantages along with excellent stiffness ad the ability to fabricate complex shapes for cost effective metal replacements.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
Water Absorption 1.4 %24 hour; ISO Test
 8.3 %ISO 62
Moisture Absorption at Equilibrium 2.3 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.0030 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ASTM Test
Tensile Strength at Break 110 MPa0.2 in/min; ASTM Test
 45.0 MPa
@Temperature 120 °C
ISO Data
 45.0 MPa
@Temperature 120 °C
ASTM Test
 115 MPa
@Temperature -40.0 °C
ASTM Test
 115 MPa
@Temperature -40.0 °C
ISO Data
Tensile Strength, Ultimate 110 MPa5mm/min; ISO 527
Elongation at Break 3.0 %0.2 in/min; ASTM Test
 3.0 %5mm/min; ISO 527
 2.0 %
@Temperature -40.0 °C
ISO Data
 2.0 %
@Temperature -40.0 °C
ASTM Test
 15 %
@Temperature 120 °C
ASTM Test
 15 %
@Temperature 120 °C
ISO Data
Tensile Modulus 5220 MPa1mm/min; ISO 527
 1445 MPa
@Temperature 120 °C
ISO Data
 2100 MPa
@Temperature 80.0 °C
ISO Data
 6370 MPa
@Temperature -40.0 °C
ISO Data
Flexural Strength 165 MPaASTM Test
 50.0 MPa
@Temperature 120 °C
ASTM Test
 200 MPa
@Temperature -40.0 °C
ASTM Test
Flexural Modulus 4300 MPaISO Data
 4650 MPaASTM Test
 995 MPa
@Temperature 120 °C
ASTM Test
Izod Impact, Notched 0.400 J/cm
@Temperature -40.0 °C
ASTM Test
 0.450 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) 5.90 kJ/m²ISO Test
Charpy Impact, Notched 0.710 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 97.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
CTE, linear, Parallel to Flow 28.0 µm/m-°CISO 11359
CTE, linear, Transverse to Flow 72.0 µm/m-°CISO 11359
Melting Point 220 °C10 K/min
 220 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 170 °CISO 75
 197 °CASTM Test
 
Processing PropertiesOriginal ValueComments
Melt Temperature 275 °CInjection molding
Mold Temperature 95.0 °CInjection molding
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueBlow Molding
ProcessingBlow molding
 Injection Molding
Special characteristicHeat stabilized or stable to heat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry)
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6

PBASF9199 / 84963

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.