MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Radiata Pine Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Test material of Chilean origin.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Permeable
Common Applications: Furniture, packaging

Key Words: Pinus radiata; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.420 g/ccGreen, Asian Origin
Density 0.318 - 0.433 g/ccat nominal specific gravity
 0.343 - 0.478 g/ccat oven-dry state
 0.378 - 0.515 g/ccat 14.3% m.c.
 0.451 g/ccNominal; at 14.3% m.c.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 2100 NSide Hardness, Green, Asian Origin
 3300 NSide Hardness, 12% Moisture, Asian Origin
Modulus of Rupture 0.0421 GPaStatic Bending, Green, Asian Origin
 0.0807 GPaStatic Bending, 12% Moisture, Asian Origin
Flexural Modulus 8100 MPaStatic Bending, Green, Asian Origin
 10200 MPaStatic Bending, 12% Moisture, Asian Origin
Compressive Strength 19.2 MPaParallel to Grain, Green, Asian Origin
 41.9 MPaParallel to Grain, 12% Moisture, Asian Origin
Machinability 100 %Good Relative to Other Wood
Shear Strength 5.20 MPaParallel to Grain, Green, Asian Origin
 11.0 MPaParallel to Grain, 12% Moisture, Asian Origin
 
Descriptive Properties
ColorYellow to pale brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Pine Wood
Northern White Pine Wood
Southern Pine Wood
European Scots Pine Wood
Lodgepole Pine Wood

PTSM010 / 71363

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.