MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Applications
Petrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with low COF.

Regulatory Status
The basic NA373 resin meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520.

Processing Techniques
Specific recommendations for processing NA373 resins can only be made when the processing conditions, equipment and end use are known.

Key Words: FDA 21 CFR 177.1520.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D1505
Thickness 1.25 milCast, as tested
 1.25 milBlown, as tested
Melt Flow 3.0 g/10 minASTM D1238
Antiblock Level 6000 ppm
Slip Level 1600 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1360 psiCast; ASTM D822
 1580 psiBlown; ASTM D822
Film Tensile Strength at Yield, TD 1350 psiCast; ASTM D822
 1550 psiBlown; ASTM D822
Film Elongation at Break, MD 200 %Blown; ASTM D822
 230 %Cast; ASTM D822
Film Elongation at Break, TD 500 %Blown; ASTM D822
 610 %Cast; ASTM D822
Elmendorf Tear Strength MD 270 gBlown; ASTM D1922
 300 gCast; ASTM D1922
Elmendorf Tear Strength TD 160 gCast; ASTM D1922
 170 gBlown; ASTM D1922
Dart Drop Test 65.0 gBlown; ASTM D1709, F50
 110 gCast; ASTM D1709, F50
Film Tensile Strength at Break, MD 2700 psiBlown; ASTM D822
 4220 psiCast; ASTM D822
Film Tensile Strength at Break, TD 2470 psiCast; ASTM D822
 2500 psiBlown; ASTM D822
1% Secant Modulus, MD 23000 psiBlown; ASTM D882
 30200 psiCast; ASTM D882
1% Secant Modulus, TD 25000 psiBlown; ASTM D882
 28600 psiCast; ASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 3.4 %Cast; ASTM D1003
 5.4 %Blown; ASTM D1003
Gloss 70 %Blown, 45°; ASTM D2457
 77 %Cast, 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 °FBlown
 500 °FCast
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQU0859 / 157480

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.