MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman BMC T44-15613 High Strength Mineral Filled Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester, Mineral Filled

Material Notes: BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing engineered phenolic materials in automotive slip-ring as well as commutator applications. Other uses are in welder tips and handles as well as structural parts.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 - 1.79 g/ccMolded
Linear Mold Shrinkage 0.0015 - 0.0025 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 30 - 40
Tensile Strength 9500 - 11500 psi
Flexural Strength 22000 - 26000 psi
Flexural Modulus 1300 - 1500 ksi
Compressive Strength 17000 - 21000 psi
Izod Impact, Notched 13.6 - 15.6 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 345 - 395 V/milshort time
Arc Resistance 188 sec
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 425 - 500 °F
Flammability, UL94 HBThis product is not currently UL listed.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 290 - 340 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC T44 High Strength Mineral Filled Molding Compound
A. Schulman BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 610 Mineral filled, glass-fiber-reinforced polyester compound
A. Schulman BMC A50-XHS High Strength Grade Molding Compound
A. Schulman BMC Super-Tough Mineral Filled, Glass Reinforced Polyester

PBMC949 / 123413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.