MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: 30% glass fiber reinforced, high thermal resistance high UV and radiation PVDF for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.95 g/ccDIN 53479
Water Absorption >= 0.040 %DIN 53495
Linear Mold Shrinkage 0.0030 cm/cm
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 58.0 MPaASTM-D638
Elongation at Break 1.2 %ASTM-D638
Tensile Modulus 1.10 GPaASTM-D790
Flexural Strength 85.0 MPaASTM-D790
Flexural Modulus 6.30 GPaASTM-D790
Izod Impact, Notched 0.850 J/cm
@Temperature 23.0 °C
ASTM-D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 175 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 3381 Polyvinylidene Fluoride (PVDF), Carbon Fiber
RTP Company RTP 3383 Polyvinylidene Fluoride (PVDF), Carbon Fiber
RTP Company RTP 3385 Polyvinylidene Fluoride (PVDF), Carbon Fiber
Zeus PVDF Tubing and Drawn Fiber
AGC Fluon® PVDF 9 White Pigmentation

PPOLYRA356 / 57618

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.