MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vitro Minerals CoreBlast™ CBM 80 100% Recycled Crushed Glass
Categories: Ceramic; Glass

Material Notes: Vitro’s CoreBlast™ Media are engineered “sandblasting” products manufactured with uniform grain size distributions from 100% Recycled Glass. CoreBlast™ can be used as a direct replacement for most hard abrasives, including silica-sand, Olivine, lava, coal slag (aka Black Beauty), and aluminum oxide. CoreBlast™ is free of crystalline silica and is approved for use in numerous federal and state government agencies, and military branches.

Information provided by Vitro Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.50 g/ccASTM C127
Bulk Density 85.0 lb/ft³ASTM C127
Moisture Absorption at Equilibrium <= 0.50 %Free; ASMT C566
Particle Mesh Size <= 80 MeshASTM C136
 80 Meshd98 top; ASTM C136
pH 10 - 11AFS 113-87-S
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 5.5
 
Component Elements PropertiesOriginal ValueComments
Al2O3 1.0 - 5.0 %
CaO 9.0 - 13 %
Fe2O3 <= 1.0 %
Lead, Pb <= 0.0040 %<40 ppm
Loss on Ignition(%) <= 1.0 %
MgO <= 1.0 %
Na2O or K2O 10 - 16 %
SiO2 70 - 80 %
SO3 <= 0.50 %
TiO2 <= 0.10 %
 
Descriptive Properties
Coloroff white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CVITRO933 / 209607

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.