Weather resistant grade. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Features: Bromine Free, Flame Retardant. Uses: Battery Cases, Electrical Parts. Forms: pellets. Processing Method: Injection Molding.Information provided by Teijin Chemicals Ltd. |