MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Solvay ThermalGraph® DKD Pitch-Based Fiber
Categories: Other Engineering Material; Composite Fibers

Material Notes: Description: ThermalGraph® DKD is a pitched-based high thermal conductivity fiber developed for thermal management applications. The fiber has a longitudinal thermal conductivity 50% higher than copper and a tensile modulus in excess of 100 Msi. The discontinuous nature of the fiber allows a free-flowing product form which can be blended and compounded with other materials. ThermalGraph DKD is especially useful in producing thermally conductive plastics and metal-matrix composites.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.15 - 2.20 g/cc
Specific Surface Area 0.40 m²/g
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 200000 psi
Tensile Modulus 689.4 - 827.28 GPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 400 - 650 W/m-K
 
Descriptive Properties
Carbon Assay99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® P-120 2K Carbon Fiber, Pitch Precursor
3M Nextel™ 550 Industrial Ceramic Fiber
3M Nextel™ 440 Industrial Ceramic Fiber
3M Nextel™ 312 Industrial Ceramic Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm

PCYTED070 / 180372

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.