MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be achieved only after conditioning, this material must be conditioned again after annealing. In addition, this conditioning occurs with a longer storage in air automatically. This polyamide has the highest hardness, rigidity, and a good resistance to wear and heat deflection temperature.

Properties:

  • high impact strength and stiffness
  • high impact and notching impact strength
  • high heat deflection temperature
  • good at dampening
  • good glide and limp home characters
  • good chemical stability against organic solvents and fuels
  • size alteration by humidity absorption must be considered
  • dimension stability, electrical and mechanical properties may become affected by absorbing moisture or water
Applications include bearing parts, gear wheels, pump parts, sliding rails, castors, and fittings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccISO 1183
Moisture Absorption at Equilibrium 1.7 %ISO 62
Water Absorption at Saturation 5.5 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ISO 868
Ball Indentation Hardness 170 MPaISO 2039
Tensile Strength at Break 100 MPaISO 527
Tensile Strength, Yield 100 MPaISO 527
Elongation at Break 5.0 %ISO 527
Modulus of Elasticity 5.00 GPaISO 527
Charpy Impact Unnotched >= 5.00 J/cm²ISO 179
Charpy Impact, Notched 0.600 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 3.00e+13 ohm-cmVDE 0303
Surface Resistivity per Square >= 1.00e+13 ohmVDE 0303
Dielectric Constant 3.6
@Frequency 1e+6 Hz
DIN 53483
Dielectric Strength 30.0 kV/mmVDE 0303
Dielectric Loss Index 0.014
@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 475 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 20.0 °C
DIN 53752
Thermal Conductivity 0.320 W/m-KDIN 52612
Melting Point 260 °CDIN EN ISO 3146
Maximum Service Temperature, Air 110 °CUL746B
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75
Minimum Service Temperature, Air -20.0 °C
Glass Transition Temp, Tg 50.0 °CDIN EN ISO 3146
Flammability, UL94 HB
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistanceyes
Bondabilityyes
CKW Resistanceno
ColorBlack
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistanceyes
Resistance Against Hot Wateryes
UV Stabilizationyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® NN-30GF/000 Polyamide 66 (Nylon 66)
GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Conditioned
Avient LubriOne™ NN-30GF/13T-2S Black Polyamide 66 (Nylon 66)
Avient Lubri-Tech™ NN-30GF/15T HS FR Nylon 6/6, Glass Filled
Overview of materials for Polyphthalamide (PPA)

PGEHR022 / 79859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.