Physical Properties | Metric | English | Comments |
---|
Solids Content | 45 - 50 % | 45 - 50 % |
Brookfield Viscosity | 5500 - 9500 cP | 5500 - 9500 cP |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 0.186 MPa @Temperature 93.0 °C | 27.0 psi @Temperature 199 °F |
| 0.207 MPa @Temperature 82.0 °C | 30.0 psi @Temperature 180 °F |
| 0.379 MPa @Temperature 66.0 °C | 55.0 psi @Temperature 151 °F |
| 0.779 MPa @Temperature 24.0 °C | 113 psi @Temperature 75.2 °F |
Shear Strength | 0.207 MPa @Temperature 93.0 °C | 30.0 psi @Temperature 199 °F |
| 0.207 MPa @Temperature 82.0 °C | 30.0 psi @Temperature 180 °F |
| 0.276 MPa @Temperature 102 °C | 40.0 psi @Temperature 216 °F |
| 0.345 MPa @Temperature 82.0 °C | 50.0 psi @Temperature 180 °F |
| 0.414 MPa @Temperature 82.0 °C | 60.0 psi @Temperature 180 °F |
| 0.517 MPa @Temperature 82.0 °C | 75.0 psi @Temperature 180 °F |
| 0.552 MPa @Temperature 82.0 °C | 80.0 psi @Temperature 180 °F |
| 0.862 MPa @Temperature 66.0 °C | 125 psi @Temperature 151 °F |
| 0.896 MPa @Temperature 66.0 °C | 130 psi @Temperature 151 °F |
| 0.965 MPa @Temperature 66.0 °C | 140 psi @Temperature 151 °F |
| 1.03 MPa @Temperature 66.0 °C | 150 psi @Temperature 151 °F |
| 1.83 MPa @Temperature 24.0 °C | 265 psi @Temperature 75.2 °F |
| 1.97 MPa @Temperature 24.0 °C | 285 psi @Temperature 75.2 °F |
| 2.10 MPa @Temperature 24.0 °C | 305 psi @Temperature 75.2 °F |
| 2.17 MPa @Temperature 24.0 °C | 315 psi @Temperature 75.2 °F |
| 3.31 MPa @Temperature 24.0 °C | 480 psi @Temperature 75.2 °F |
| 7.58 MPa @Temperature -37.0 °C | 1100 psi @Temperature -34.6 °F |
Peel Strength | 0.877 kN/m @Temperature -37.0 °C, Time 1.81e+6 sec | 5.00 pli @Temperature -34.6 °F, Time 504 hour |
| 1.75 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec | 10.0 pli @Temperature 151 °F, Time 504 hour |
| 1.75 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec | 10.0 pli @Temperature 180 °F, Time 504 hour |
| 2.63 kN/m @Temperature 24.0 °C, Time 1.81e+6 sec | 15.0 pli @Temperature 75.2 °F, Time 504 hour |
| 3.51 kN/m @Temperature 24.0 °C, Time 605000 sec | 20.0 pli @Temperature 75.2 °F, Time 168 hour |
| 3.51 kN/m @Temperature 24.0 °C, Time 1.21e+6 sec | 20.0 pli @Temperature 75.2 °F, Time 336 hour |
| 4.38 kN/m @Temperature 24.0 °C, Time 86400 sec | 25.0 pli @Temperature 75.2 °F, Time 24.0 hour |
| 5.26 kN/m @Temperature 24.0 °C, Time 432000 sec | 30.0 pli @Temperature 75.2 °F, Time 120 hour |
| 6.14 kN/m @Temperature 24.0 °C, Time 259000 sec | 35.0 pli @Temperature 75.2 °F, Time 72.0 hour |
|
Descriptive Properties |
---|
Appearance | Blue (Wet), Green (Dry) |
Base | Polychloroprene |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view