Notes: Medalist MD-12368 is a high performance thermoplastic elastomer intended for use in healthcare and medical applications. Medalist MD-12368 is a medium hardness, low density, clear grade designed suitable for injection molding, extruded tubing, and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Abrasion Resistant, Autoclave Sterilizable; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Flexibility; Good Moldability; Good Processability; Good Sterilizability; Good Strength; Good Tear Strength; Good Toughness; Halogen Free; Low Density; Medium Hardness; Radiation (Gamma) Resistant; Radiation Sterilizable; Resilient Uses: Closures; Diaphragms; Disposable Hospital Goods; Flexible Grips; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement; Tubing Agency Ratings: ISO 10993 Part 5; ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion; Injection Molding Information provided by Teknor Apex |