MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound RC006 Polyamide 66 (Nylon 66) (Asia)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP THERMOCOMP RC006 compound is based on Nylon 6/6 resin containing 30% carbon fiber. Added features of this grade include: Electrically Conductive.

Features: High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ISO 1183
 1.28 g/cc0.0462 lb/in³ASTM D792
Moisture Absorption 0.600 %0.600 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.00080 cm/cm0.00080 in/in24hrs; ISO 294
 0.0010 cm/cm0.0010 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0056 cm/cm0.0056 in/in24hrs; ISO 294
 0.0060 cm/cm0.0060 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 266 MPa38600 psiASTM D638
 271 MPa39300 psiISO 527
Elongation at Break 1.7 %1.7 %ASTM D638
 1.9 %1.9 %ISO 527
Tensile Modulus 22.3 GPa3230 ksi1 mm/min; ISO 527
 27.78 GPa4029 ksi50 mm/min; ASTM D638
Flexural Strength 406 MPa58900 psiASTM D790
 412 MPa59800 psiISO 178
Flexural Modulus 18.75 GPa2719 ksiASTM D790
 21.02 GPa3049 ksiISO 178
Izod Impact Notched 96.0 J70.8 ft-lbASTM D256
Izod Impact, Unnotched 10.14 J/cm19.00 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 67.0 kJ/m²31.9 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 15.0 J11.1 ft-lbpeak; ASTM D3763
Impact Test 3.00 J2.21 ft-lbMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.460.46ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.360.36ASTM D3702 Modified: Manual
K (wear) Factor 40.3 x 10-8 mm³/N-M20.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  10.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
6.00 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 11.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
6.39 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  48.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
27.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 48.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
27.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
@Thickness 3.20 mm
502 °F
@Thickness 0.126 in
unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81829 / 289776

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.