MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman 1840A Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Polyethylene 1840A is a low-density formulation with no slip or antiblock. It is suggested for injection molding applications requiring good stiffness, gloss, good processability or layflat properties.

Applications/Uses

  • Food cooking applications
  • Food-contact applications
  • Key Attributes
  • Good processability
  • Good stiffness
  • Use in injection molding applications
  • Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.921 g/ccASTM D4883
    Melt Flow 2.25 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 12.0 MPa500 mm/min; ASTM D638
    Tensile Strength, Yield 10.8 MPa500 mm/min; ASTM D638
    Elongation at Break 380 %500 mm/min; ASTM D638
    Flexural Modulus 0.269 GPa
    @Strain 2 %
    Secant; 12.7 mm/min. (0.5 in./min.); ASTM D790
     
    Thermal PropertiesOriginal ValueComments
    Vicat Softening Point 94.0 °CASTM D1525
    Brittleness Temperature <= -73.0 °CASTM D746

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade
    LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene
    Bamberger Polymers Bapolene® 1030 Low Density Polyethylene Extrusion/Injection Resin
    Armacell OleTex® BKJN 200 LDPE Foam
    Armacell OleTex® BCJN 200 EVA/LDPE Foam

    PE9150 / 35207

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.