MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Chemlon® 60GF3H Nylon 6, Conditioned, 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Notes: 60GF3H is a 15% glass fiber reinforced, heat stabilized nylon 6 that offers good mechanical performance and improved endurance at elevated service temperatures.

Availability: Europe

Fillers/Reinforcement: Carbon Fiber, 15% Filler by Weight

Additive: Heat Stabilizer

Features: Heat Stabilized

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.5 %2.5 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.010 - 0.016 cm/cm0.010 - 0.016 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 70.3 MPa10200 psiISO 527-2
Flexural Strength 84.8 MPa12300 psiISO 178
Flexural Modulus 2.50 GPa363 ksiISO 178
Charpy Impact, Notched 2.10 J/cm²10.0 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Strength 7.87 kV/mm
@Thickness 3.00 mm
200 kV/in
@Thickness 0.118 in
IEC 60243-1
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 280 °C446 - 536 °F
Middle Barrel Temperature 230 - 280 °C446 - 536 °F
Front Barrel Temperature 230 - 280 °C446 - 536 °F
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 20.0 hour20.0 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0379 / 236870

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.