MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals

(Viewing data as-entered. Click here to return)
Nickel, Ni
Categories: Metal; Nonferrous Metal; Nickel Alloy; Pure Element

Material Notes: This entry is for pure Ni.

Nickel based alloys are the mainstay of many high performance markets in which corrosion resistance and/or heat resistance is required. Example applications include furnace components, chemical processing vessels, exchangers, and piping, high temperature aerospace components, nuclear reactors, extreme service pumps, turbines, pulp and paper production, and pollution control.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.88 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 58.69341995
Atomic Number 28
Thermal Neutron Cross Section 4.8 barns/atom
X-ray Absorption Edge 1.488 ÅK
 12.267 ÅLI
 14.135 ÅLII
 14.4476 ÅLIII
Electrode Potential -0.250 V
Electronegativity 1.91Pauling
Ionic Radius 0.690 ÅCrystal Ionic Radius for Valence +2
Electrochemical Equivalent 1.0945 g/A/h
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 45.0 MPaAnnealed
 317 MPaTypical
Tensile Strength, Yield 59.0 MPaTypical
Elongation at Break 30 %Annealed
Modulus of Elasticity 207 GPa
Poissons Ratio 0.31
Shear Modulus 76.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000640 ohm-cm
Magnetic Permeability 1240mu(max) with B=1900G
Curie Temperature 358 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 305.6 J/g
Heat of Vaporization 5862 J/g
CTE, linear 13.1 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 60.7 W/m-K
Melting Point 1455 °C
Boiling Point 2913 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.080
@Temperature 200 - 400 °C
polished total spectrum
 0.19
@Temperature 1000 °C
unoxidized
Reflection Coefficient, Visible (0-1) 0.413300 nm spectral
 
Component Elements PropertiesOriginal ValueComments
Nickel, Ni 100 %
 
Descriptive Properties
CAS Number7440-02-0

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum, Al
Iron, Fe
Gold, Au
Titanium, Ti
Copper, Cu; Annealed

AMENi00 / 71

Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.