MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient OnFlex™ V 3040D-S0093 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolefin phase with a cross-linked EPDM phase dispersed within it. This range of compounds are specially formulated to provide the melt strength and processability required for blow-moulding processes. In addition to this, OnFlex™-V 3000 series thermoplastic elastomer compounds provide excellent colourability (low yellowness), good mechanical properties, excellent flexibility over a wide temperature range, a wide hardness range, and good hydrocarbon, heat ageing and weather resistance.

Properties are measured using injection molded plaques.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40ISO 868
Tensile Strength at Break 15.7 MPaISO 37
Tensile Stress at Strain 7.60 MPa
@Strain 100 %
ISO 37
 9.30 MPa
@Strain 300 %
ISO 37
Elongation at Break 570 %ISO 37
Compression Set 38 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
 60 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 61 %
@Temperature 100 °C,
Time 79200 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 230 °C
Mold Temperature 30.0 - 60.0 °C
Drying Temperature 80.0 °C
Dry Time 3.00 hour
 
Descriptive Properties
FeaturesGeneral Purpose
FormsPellets
Generic MaterialTPE
Generic Material TypeThermoplastic Vulcanizate (TPV)
Generic NameThermoplastic Elastomer (TPE)
Injection RateFast
Processing MethodBlow Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Neoprene FB Polychloroprene Rubber
ExxonMobil LD 150013.BA Low Density Polyethylene Resin (European Grade)
Dow Nordel® IP 4520 Molded Golf Grip
Avient Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE)
Avient Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE)

PH0POL0767 / 145336

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.