MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® eXten D 218CR V33 BLACK Nylon Blend, PA 6.10, 66, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Description: TECHNYL® eXten D 218CR V33 BLACK is a glass fiber reinforced grade based on blend Polyamide 6.10 and Polyamide 66, for Injection Moulding. This product is available in Black.

Key Properties: Salt crack resistance; Excellent glycol resistance; Good thermal properties; Best in class processing

Benefits: The product shows outstanding resistance to hydrolysis and chemical resistance to long life automotive coolants. It also offers an excellent crack resistance to calcium chloride road salts, good injection process ability, high surface aspect quality, and high overall mechanical and thermal properties.

Applications: It is used in automotive industry, for cooling circuit components such as Radiator end tanks or Thermostat housing. Moreover it is notably recommended for automotive applications exposed to aggressive chemicals (especially to calcium chloride road salts) such as wheel speed sensors.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183/A
Water Absorption 0.30 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 1.3 %ISO 1110
Water Absorption at Saturation 3.6 %ISO 62
Viscosity Test 130 cm³/gISO 307
Linear Mold Shrinkage, Flow 0.0020 cm/cm
Linear Mold Shrinkage, Transverse 0.010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 196 MPaISO 527 Type 1A
Elongation at Break 3.3 %ISO 527 Type 1A
Tensile Modulus 11300 MPaISO 527 Type 1A
Flexural Strength 280 MPaISO 178
Flexural Modulus 10150 MPaISO 178
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 94.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.80 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Strength 34.0 kV/mmIEC 60243
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 - 260 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 225 °CISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 218 °CISO 75/Af
Flammability, UL94 HB
@Thickness 0.400 mm
ISO 1210
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 290 °CCompression zone
 280 - 295 °CMixing zone
Feed Temperature 260 - 280 °C
Drying Temperature 120 °C
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY
Domo TECHNYL® C 216 V40 PA6, 40% glass fiber, DRY
Avient Bergamid™ A70 G15 HW TM-Z Polyamide 66 (Nylon 66)
Domo TECHNYL® AR 218 V25 Nylon 66, 25% glass fiber, DRY
Domo TECHNYL® A 218 Natural PA 66, Dry

PSOLVAY817 / 218545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.