MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics WDS® Flexipor® Porextherm
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: WDS® Flexipor® is a microporous insulation material which has an extremely low thermal conductivity coefficient giving it very good insulating properties. WDS® Flexipor® is produced with temperature resistant soluble paper on both sides which is then wrapped in PE film, this enhances the flexibility purposes of the product. WDS® Flexipor® is designed with no gaps. This has a signicant improvement on insulation due to decrease in heat transition. WDS® Flexipor® consists of inorganic silicates. The main constituent is fumed silica; the other components are opacifiers to minimize infrared radiation and reinforce glass filaments. WDS® Flexipor® (core material) is not flammable and meets the requirements of IMO FTPC and DIN EN 13501-1, part 1 class A1.

Application: Tried and tested applications for WDS® Flexipor® include back-up insulation in the steel and non-ferrous metals industry.

Typical applications: WDS® Flexipor® is also successfully used as insulation material in the following areas: Heat treatment systems for metals, Heat treatment systems for glass, Fire protection equipment, Electronic devices, Metrology and instrumentation, Plant construction parts. Parts in the automotive industry, Chimneys, pipes and diesel exhaust systems.

Information provided by Morgan Advanced Materials

Key Words: Porextherm
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 - 0.350 g/ccnominal
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 0.607 MPaat RT; ASTM 0165
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.220 BTU/lb-°F
@Temperature 700.0 °C
DIN 51007
Thermal Conductivity 0.0220 W/m-K
@Temperature 22.5 °C
ASTM C177
 0.0230 W/m-K
@Temperature 200 °C
ASTM C177
 0.0270 W/m-K
@Temperature 400 °C
ASTM C177
 0.0340 W/m-K
@Temperature 600 °C
ASTM C177
 0.0460 W/m-K
@Temperature 800 °C
ASTM C177
Shrinkage 0.60 %
@Treatment Temp. 1000 °C,
Time 43200 sec
exposed at single side, ASWW 906-00
 1.7 %
@Treatment Temp. 950 °C,
Time 86400 sec
full soak
 3.6 %
@Treatment Temp. 1000 °C,
Time 86400 sec
full soak
 
Component Elements PropertiesOriginal ValueComments
Other 5.0 %
 45 %ZrSiO4
SiO2 50 %
 
Descriptive Properties
Classification Temperature (°C)1100
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6121 / 202905

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.