Made by emulsion polymerization for plastisol preparation.
MAIN APPLICATIONS
Spread coating :
- artificial leather compact layer
- flooring top coat.
ADVANTAGES
- Matt appearance in flooring to coat.
- Good viscosity stability on storage. Information provided by SolVin. SolVin is a predecessor company to Inovyn. |