MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Angst+Pfister APSOplast® PE-UHMW FR Flame-retardant
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: PE-UHMW FR is a flame-retardant material which also has anti-static and UV-stable properties in conjunction with the proven properties of PE-UHMW.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³DIN EN ISO 1183-1
Moisture Absorption <= 0.0500 %<= 0.0500 %50 % r.h.; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363DIN EN ISO 868
Tensile Strength, Yield 22.0 MPa3190 psi50 mm/min; DIN EN ISO 527
Elongation at Break >= 200 %>= 200 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 0.700 GPa102 ksi1 mm/min; DIN EN ISO 527
Charpy Impact, Notched NBNBDIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1000 ohm-cm>= 1000 ohm-cmIEC 60093
Surface Resistance <= 10000 ohm<= 10000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 - 230 µm/m-°C83.3 - 128 µin/in-°FDIN 53752
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Melting Point 135 °C275 °FISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C176 °Flong term
 130 °C266 °Fshort term
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C174 °FDIN EN ISO 75
Minimum Service Temperature, Air -250 °C-418 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP010 / 250508

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.