MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Persian Gulf Polymer LDPE – LD 2426F8
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: It is delivered in pellet form. Application: High impact strength, Freezer films, Lamination film, Shopping bags. Feature: Homo-polymer, Food Grade. Additives: Slip agent, Anti-block.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 - 0.926 g/cc0.0333 - 0.0335 lb/in³ISO 1183 (A)
Melt Flow 0.70 - 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 - 0.90 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiISO 527
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiISO 527
Film Elongation at Break, MD >= 200 %>= 200 %ISO 527-1,-3
Film Elongation at Break, TD >= 500 %>= 500 %ISO 527-1,-3
Tensile Impact Strength 30.0 kJ/m²14.3 ft-lb/in²ASTM D4272
Coefficient of Friction 1.01.0ASTM D1894
Tear Strength 30.0 kN/m171 pliMD; ISO 6383-2
 30.0 kN/m171 pliTD; ISO 6383-2
Dart Drop Test >= 140 g>= 0.309 lbASTM D1709
 
Optical PropertiesMetricEnglishComments
Haze <= 8.0 %<= 8.0 %ASTM D1003 A
Gloss 45 %45 %DIN 67350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI959 / 250363

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.