SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands of standard UL 94 category HB, on request category V0 is available. The glass content is on a level that combines good mouldability with good mechanical properties regarding strength and stiffness.Information Provided by Menzolit |