MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Novec™ 72DA Engineered Fluid
Categories: Fluid

Material Notes: 3M™ Novec™ 72DA is ideal for flux removal and vapor degreasing operations. It is non-flammable and low in toxicity which makes it an ideal replacement for chlorinated solvents such as Trichloroethylene (TCE) and for n-propyl bromide (nPB).

Feature and Benefits:

  • Non-flammable
  • Non-conductive
  • Low toxicity
  • Low Global Warming Potential (GWP)
  • Zero ozone depletion potential
  • Low surface tension penetrates tight spaces for improved cleaning
  • Excellent for removal of ionic contamination

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³Liquid
Viscosity 0.40 cP0.40 cP
Vapor Pressure 0.480 bar360 torr
Surface Tension 18 dynes/cm18 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 251.2 J/g108.1 BTU/lb
Boiling Point 44.0 °C111 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 7100DL Engineered Fluid
3M Novec™ 7100 Engineered Fluid
3M Novec™ 7000 Engineered Fluid
3M Novec™ 649 Engineered Fluid
3M Novec™ 71DA Engineered Fluid

PMM33111 / 167858

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.