MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES HiFill FR® PA6 GF13 FR 13% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight

Additive: Heat Stabilizer and Lubricant

Features: Flame Retardant, Heat Stabilized and Lubricated

RoHS Compliance: RoHS Compliant

Appearance: Black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccASTM D792
Water Absorption 0.90 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 16000 psiASTM D638
Elongation at Break 4.2 %ASTM D638
Flexural Strength 22000 psiASTM D790
Flexural Modulus 700000 psiASTM D790
Izod Impact, Notched 1.70 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohmASTM D257
Dielectric Strength 400 V/milMethod A (Short-Time); ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 420 °FUnannealed; ASTM D648
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Matrixx FP63E13 13% Glass Filled Nylon 6
LG Chemical LUMID GP2130AE PA6+GF13%, General Purpose
Techmer ES HiFill® PA6 GF13 L 13% Glass Filled
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose
Techmer ES HiFill FR® PA6 GF13 FR-N BK 13% Glass Filled

PTPC0666 / 136604

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.