MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AGC AFLAS® SZ TFE/P/VdF Fluoroelastomer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: AFLAS® SZ/SP are terpolymers containing tetrafluoroethylene, propylene, and a small amount of vinylidene fluoride used as a cure site monomer. This combination gives AFLAS® SZ/SP a good balance of chemical resistance and improved processability when compared to AFLAS® 100/150 dipolymers. AFLAS® SZ is bisphenol-cured, while AFLAS® SP is peroxide-cured. Both polymers are categorized in ASTM D 1481-01 as class FKM, type four.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Mooney Viscosity 67
@Temperature 100 °C
ML1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
Tensile Strength at Break 19.6 MPaASTM D638
Elongation at Break 240 %ASTM D638
Compression Set 35 %
@Temperature 200 °C
70h
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -3.00 °C
 
Descriptive Properties
Fluorine Content %55

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material
Avient Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE)
ATG s.r.l. FVMQ Fluorosilicone Rubber
ATG s.r.l. EPM Ethylene-Propylene Copolymer

PAGC28 / 22987

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.