MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Nouryon Thioplast G4 Liquid polysulfide polymer with thiol end groups
Categories: Other Engineering Material

Material Notes: The low viscosity combined with Thioplast's unique combination of features like chemical resistance and low-temperature flexibility appeals to high-performance coating manufacturers of all industry branches to protect metal or concrete surfaces, floors, or pipelines. Formulators tailor properties like pot-life, tensile strength, adhesion and elongation at break by choosing from various compatible plasticizers, fillers and other additives. The viscosity, degree of branching and SH content can easily be adjusted by blending this grade with others to generate your tailored Thioplast polysulfide.

CAS number: 68611-50-7

Applications: Thioplast G4 is used as reactive diluent in Thioplast G based sealants to formulate low viscos, flexible and highly elastic sealants being used in aerospace and construction applications with best performance in high Nobel Gas retention and low moisture vapor permeability. Additionally, Thioplast G4 is used as highly reactive partner in Amine cured Epoxies (like Bisphenol (A, F, AF) DGE and Novolac) to adapt and optimize tensile- / impact strength and elasticity (brittleness). Support on stoichiometric calculation to cure Epoxies with Thioplast G4 is available on request.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.70 %
Viscosity <= 1.3 cP
Molecular Weight <= 1100 g/mol
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 230 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.35 %
 
Descriptive Properties
AppearanceBrownish liquid polymer
Content0.01-0.1 %Free sulfur
 2.0 mol%Branching, calculated on mol% TCP
 6.0-7.0 %SH content, related to viscosity/Molecular weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY944 / 286467

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.