MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: IFs932-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.

NOVA Chemicals' polyethylene resins are biologically and chemically inert.

Features: Excellent balance of stiffness and toughness to meet application requirements, Low viscosity for exceptional processability yielding shorter cycle times and energy savings, Increases opportunities for light-weighting of lid designs, Low warpage for improved part quality and reliability, Superior organoleptic properties, Excellent contact clarity properties

Additives: Antioxidant, Mold release

Applications: Lids, for non-frozen, thin wall, food packaging containers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.932 g/ccASTM D 792
Melt Flow 150 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
Spiral Flow 50.8 cmNOVA Chemicals snake flow number
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D 2240
Tensile Strength at Break 10.0 MPaRate of 50 mm/min; ASTM D 638
Tensile Strength, Yield 16.0 MPaRate of 50 mm/min; ASTM D 638
Elongation at Break 35 %Rate of 50 mm/min; ASTM D 638
Elongation at Yield 11 %Rate of 50 mm/min; ASTM D 638
Tensile Modulus 0.700 GPa1% Secant; ASTM D 638
Flexural Modulus, 1% Secant 580 MPaASTM D 790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 98.0 °CASTM 1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
Aaron Industries AVPE HD 300-3 Virgin Polyethylene
Aaron Industries AAROLENE® ARPE HD 300-2 High Density Polyethylene Compounded Resin
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE)

PNOV778 / 108903

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.