MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) BLUESIL™ EMUL E1P Silicone Emulsion -Release Agent
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: BLUESIL™ EMUL E1P is a general purpose, nonionic aqueous silicone emulsion.

Applications:

  • Mold release agent for technical rubber, tires, plastics and foundry products
  • Water repellent and release agent for industrial glassware
  • Additive in maintenance products: floor and furniture polishes, products for leather maintenance
  • Textile lubrication, sizing and finishing agent
  • Tack modifier for emulsion adhesives
  • Slip additive for curable release coatings

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
Solids Content 40 %
pH 7.0
Viscosity 350 cP
Storage Temperature 2.00 - 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceMilky white liquid
DiluentsWater, with hardness lower than 250 ppm
Emulsifier typeNon-ionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) SILCOLAPSE® 422 Silicone Emulsion

PBLUST124 / 191107

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.