MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DIC FZ-3600-D5 Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Glass fiber and mineral filled (Branched PPS.) GF/Filler Standard.

Information provided by DIC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.89 g/cc0.0683 lb/in³ISO 1183
Water Absorption 0.010 %
@Temperature 23.0 °C,
Time 86400 sec
0.010 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 145 MPa21000 psiISO 527-1,2
Elongation at Break 1.0 %1.0 %ISO 527-1,2
Tensile Modulus 20.5 GPa2970 ksiISO 527-1,2
Flexural Strength 235 MPa34100 psiISO 178
Flexural Modulus 19.5 GPa2830 ksiISO 178
Flexural Strain at Break 1.4 %1.4 %ISO 178
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²ISO 179/eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/eA
Coefficient of Friction, Dynamic 0.350.35P= 150 kPa, V=0.3 m/s, PPS vs carbon steel
Coefficient of Friction, Static 0.350.35P= 150 kPa, V=0.3 m/s, PPS vs carbon steel
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm
@Thickness 1.00 mm
559 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  15.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F
@Temperature -58.0 - 122 °F
ISO 11359-2
 15.0 µm/m-°C
@Temperature 100 - 200 °C
8.33 µin/in-°F
@Temperature 212 - 392 °F
ISO 11359-2
CTE, linear, Transverse to Flow  25.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
13.9 µin/in-°F
@Temperature -58.0 - 122 °F
ISO 11359-2
 70.0 µm/m-°C
@Temperature 100 - 200 °C
38.9 µin/in-°F
@Temperature 212 - 392 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 275 °C527 °FISO-75-1,2
Flammability, UL94 V-0
@Thickness 0.730 mm
V-0
@Thickness 0.0287 in
UL file No. E53829
 
Processing PropertiesMetricEnglishComments
Processing Temperature 300 - 340 °C572 - 644 °FCylinder Temperature
Mold Temperature 130 - 150 °C266 - 302 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDIC9907 / 248338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.