System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lehvoss LUVOCOM® 3F PA
HT
® KK 50056 BK FR Nylon, Ceramic Sphere Filled, for Additive Manufacturing
Categories:
Polymer
;
3D Printing/Additive Manufacturing Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
High Temperature Nylon
Material Notes:
High-temperature polyamide with ceramic spheres, flame retardant, black
Main features: Easy to print. No warping. Meets EN 45545.
Information provided by Lehmann & Voss & Co.KG
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.40
g/cc
ISO 1183-3
Water Absorption
<= 0.300 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage
0.000
-
0.00100
cm/cm
DIN 16742
Mechanical Properties
Original Value
Comments
Tensile Strength
55.0
MPa
50 mm/min; ISO 527
Elongation at Break
1.70 %
50 mm/min, Fmax; ISO 527
Tensile Modulus
5.50
GPa
1 mm/min; ISO 527
Electrical Properties
Original Value
Comments
Surface Resistance
<=
1.00e+9
ohm
Ronde 60x4mm; DIN EN 62631-3-2
Insulation Resistance
<=
1.00e+9
ohm
strip electrode R25; DIN EN 62631-3-3
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
120
°C
@Time 7.20e+7 sec
Continuous; IEC 60216
160
°C
@Time 720000 sec
during lifetime
Deflection Temperature at 1.8 MPa (264 psi)
90.0
°C
80x10x4mm; ISO 75
Flammability, UL94
V-0
@Thickness 1.59 mm
printed specimen @0.4 mm
Processing Properties
Original Value
Comments
Nozzle Temperature
250
-
290
°C
Zone 1
260
-
300
°C
Zone 2
260
-
300
°C
Zone 3
260
-
300
°C
Drying Temperature
120
°C
@Time 14400 - 21600 sec
Vacuum
130
°C
@Time 21600 - 28800 sec
Dehumidifying
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PLUU8728 / 325112
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.