MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ductile Iron grade 60-40-18, low temperature service
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Carbon represents the total carbon in the listed composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. For example, 60-40-18 ductile iron is specified to have a minimum tensile strength of 60 ksi (414 MPa), a yield strength of 40 ksi (276 MPa) and an elongation of 18%. Ferritic, may be annealed. Applications include shock resistant parts, low temperature service, machine components subject to shock and fatigue loads.

Key Words: UNS F32800, ASTM A536-72, MIL-I-11466B(MR), ferritic, shock resistant parts
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.10 - 7.20 g/ccTypical value of ductile iron
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 414 MPa
Tensile Strength, Yield >= 276 MPa
Elongation at Break 18 %In 50 mm.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 3.6 - 3.8 %
Cerium, Ce 0.0050 - 0.20 %
Chromium, Cr 0.030 - 0.070 %
Copper, Cu 0.15 - 1.0 %
Iron, Fe 90.738 - 94.175 %
Magnesium, Mg 0.030 - 0.060 %
Manganese, Mn 0.15 - 1.0 %
Molybdenum, Mo 0.010 - 0.10 %
Nickel, Ni 0.050 - 0.20 %
Phosphorus, P <= 0.030 %
Silicon, Si 1.8 - 2.8 %
Sulfur, S <= 0.0020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ductile Iron grade 60-40-18
Ductile Iron grade 65-45-12
Ductile Iron grade 80-55-06
Ductile Iron tension grade 60-40-18
Ductile Iron grade 80-60-03

MDFE03 / 12000

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.