Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Low Gloss; Low Temperature Flexibility Uses:Communication Wire Jacketing; Patch Cord Jacketing Form: Pellets Processing Method: Extrusion Information provided by Teknor Apex |