MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyChem Alloy PolyGard 3005R
Categories: Polymer

Material Notes: PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the physical properties. Other benefits include the elimination of sink marks and an improved surface quality. For foamed extrusions, PolyFoam used in combination with a gas blowing agent improves the efficiency of the physical agent, reducing of gas usage, part weight, and often scrap. PolyFoam products come in a uniform pelletized shape and are available with endothermic blowing agents, exothermic blowing agents, or both.

Key Words: PolyChem Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 - 1.30 g/cc1.10 - 1.30 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 38 - 4238 - 42
Elongation at Yield 110 - 130 %110 - 130 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 250 °C<= 482 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyChem Alloy PolyShield 1346

PPC240 / 56071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.