MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultrason® E 2010 C6 30% Carbon Filled
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone, Carbon Fiber Reinforced

Material Notes: Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatures of up to 200 °C.

Excellent properties: very high stiffness, very constant mechanical properties, low and constant thermal expansion = dimensionally stable and excellent creep behavior

Potential applications: Substitution of metal, using the advantages of thermoplastic materials (e.g. realization of complex designs by injection-molding), substitution of PEEK for applications with a maximum of 200 °C, parts with antistatic requirements and parts with electrically conductive requirements

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 - 0.800 g/cc0.0253 - 0.0289 lb/in³
Density 1.47 g/cc0.0531 lb/in³ISO 1183
Water Absorption <= 1.7 %<= 1.7 %Equilibrium; ISO 62
Moisture Absorption at Equilibrium 0.60 %0.60 %23°C; 50% RH; ISO 62
Viscosity Test 56 cm³/g0.56 dl/gISO 1628
Linear Mold Shrinkage, Flow 0.0015 cm/cm0.0015 in/inISO 294
Linear Mold Shrinkage, Transverse 0.0035 cm/cm0.0035 in/inISO 294
Melt Flow  >= 22.05 g/10 min
@Load 10.0 kg,
Temperature 360 °C
>= 22.05 g/10 min
@Load 22.0 lb,
Temperature 680 °F
ISO 1133
 >= 45 g/10 min
@Load 10.0 kg,
Temperature 400 °C
>= 45 g/10 min
@Load 22.0 lb,
Temperature 752 °F
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 227 MPa
@Load 36.5 kg,
Time 30.0 sec
32900 psi
@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength at Break 185 MPa26800 psi5 mm/min; ISO 527-2
Tensile Strength, Yield 185 MPa26800 psi50 mm/min; ISO 527-2
Elongation at Break 1.5 %1.5 %5mm/min; ISO 527-2
Elongation at Yield 1.5 %1.5 %50 mm/min; ISO 527-2
 0.21 %
@Time 3600 sec,
Pressure 50.0 MPa
0.21 %
@Time 1.00 hour,
Pressure 7250 psi
ISO 899
 0.23 %
@Pressure 50.0 MPa,
Time 360000 sec
0.23 %
@Pressure 7250 psi,
Time 100 hour
ISO 899
 0.24 %
@Pressure 50.0 MPa,
Time 3.60e+6 sec
0.24 %
@Pressure 7250 psi,
Time 1000 hour
ISO 899
 0.38 %
@Time 3600 sec,
Pressure 70.0 MPa
0.38 %
@Time 1.00 hour,
Pressure 10200 psi
ISO 899
 0.40 %
@Pressure 70.0 MPa,
Time 360000 sec
0.40 %
@Pressure 10200 psi,
Time 100 hour
ISO 899
 0.40 %
@Pressure 70.0 MPa,
Time 3.60e+6 sec
0.40 %
@Pressure 10200 psi,
Time 1000 hour
ISO 899
 0.50 %
@Time 3600 sec,
Pressure 90.0 MPa
0.50 %
@Time 1.00 hour,
Pressure 13100 psi
ISO 899
 0.55 %
@Pressure 90.0 MPa,
Time 360000 sec
0.55 %
@Pressure 13100 psi,
Time 100 hour
ISO 899
 0.58 %
@Pressure 90.0 MPa,
Time 3.60e+6 sec
0.58 %
@Pressure 13100 psi,
Time 1000 hour
ISO 899
 0.60 %
@Time 3600 sec,
Pressure 110 MPa
0.60 %
@Time 1.00 hour,
Pressure 16000 psi
ISO 899
 0.70 %
@Time 360000 sec,
Pressure 110 MPa
0.70 %
@Time 100 hour,
Pressure 16000 psi
ISO 899
 0.75 %
@Pressure 110 MPa,
Time 3.60e+6 sec
0.75 %
@Pressure 16000 psi,
Time 1000 hour
ISO 899
 0.80 %
@Time 3600 sec,
Pressure 130 MPa
0.80 %
@Time 1.00 hour,
Pressure 18900 psi
ISO 899
 0.90 %
@Time 360000 sec,
Pressure 130 MPa
0.90 %
@Time 100 hour,
Pressure 18900 psi
ISO 899
 0.98 %
@Pressure 130 MPa,
Time 3.60e+6 sec
0.98 %
@Pressure 18900 psi,
Time 1000 hour
ISO 899
Tensile Modulus  >= 13.0 GPa
@Temperature 200 °C
>= 1890 ksi
@Temperature 392 °F
 >= 20.0 GPa
@Temperature 150 °C
>= 2900 ksi
@Temperature 302 °F
 >= 21.0 GPa
@Temperature 100 °C
>= 3050 ksi
@Temperature 212 °F
 >= 22.0 GPa
@Temperature 50.0 °C
>= 3190 ksi
@Temperature 122 °F
ISO 527-2
Shear Modulus  0.200 GPa
@Temperature 225 °C
29.0 ksi
@Temperature 437 °F
ISO 6721
 0.900 GPa
@Temperature 200 °C
131 ksi
@Temperature 392 °F
ISO 6721
 0.950 GPa
@Temperature 100 °C
138 ksi
@Temperature 212 °F
ISO 6721
 1.00 GPa
@Temperature 50.0 °C
145 ksi
@Temperature 122 °F
ISO 6721
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180/A
 7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179/1eU
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.750 J/cm²3.57 ft-lb/in²ISO 179/1eA
 0.650 J/cm²
@Temperature -30.0 °C
3.09 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.9 ohm-cm1.9 ohm-cmIEC 60093
Surface Resistance >= 1000 ohm>= 1000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  4.00 µm/m-°C
@Temperature 23.0 - 80.0 °C
2.22 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
 4.00 µm/m-°C
@Temperature 140 - 180 °C
2.22 µin/in-°F
@Temperature 284 - 356 °F
ISO 11359-1/-2
Maximum Service Temperature, Air 220 °C428 °Fshort cycle operations
Deflection Temperature at 1.8 MPa (264 psi) 225 °C437 °FISO 75-2
Glass Transition Temp, Tg 225 °C437 °FISO 11357-1/-2
Decomposition Temperature >= 400 °C>= 752 °F
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Ignition Temperature 580 - 600 °C1080 - 1110 °FDIN 54836
 
Processing PropertiesMetricEnglishComments
Melt Temperature 350 - 390 °C662 - 734 °FInjection molding/extrusion
 370 °C698 °FOptimal
Mold Temperature 150 - 190 °C302 - 374 °FInjection molding
 170 °C338 °FOptimal
Drying Temperature 140 °C284 °F
Dry Time 4 hour4 hour
 
Descriptive Properties
ColorBlack
Commercial StatusNorth America and Europe
Primary Processing TechniqueInjection Molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2299 X 115090 B Polyetheretherketone (PEEK), Carbon Nanotube - Electrically Conductive
RTP Company RTP 2287 HEC Polyetheretherketone (PEEK); Nickel-Coated Carbon Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 2263 Polyetheretherketone (PEEK), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company RTP 1499 P X 125056 A Polyphenyl Sulfone (PPSU) Stainless Steel Fiber - EMI/RFI Shielding
RTP Company RTP 2283 HEC Polyetheretherketone (PEEK), Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection - Electrically Conductive

PBASG0170 / 131803

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.