MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil SpectraSyn Elite™ 150 Metallocene Polyalphaolefin (mPAO) Fluid
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Product Description: SpectraSyn Elite™ metallocene Polyalphaolefin (mPAO) basestock is an advanced high viscosity (Hi-Vis) Polyalphaolefin (PAO). SpectraSyn Elite™ mPAO utilized metallocene catalyst technology. SpectraSyn Elite™ mPAO basestock offers performance characteristics not available with conventional PAO, such as improved viscosity index (VI), shear stability and low temperature performance in finished lubricants optimized to address formulators’ toughest lubrication challenges.

Appearance: Bright & Clear

Availability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.849 g/cc
@Temperature 15.6 °C
0.0307 lb/in³
@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 206206Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 1705 cSt1705 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 156 cSt156 cStASTM D445
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10[mg KOH/g]; ASTM D974 (mod)
 
Thermal PropertiesMetricEnglishComments
Pour Point -32.8 °C-27.0 °FASTM D5950/D97
Flash Point 282 °C540 °FCOC; ASTM D6304 (mod)
 
Descriptive Properties
Color<0.5ASTM D1500
CompositionWater<50 ppm, ASTM D6304 (mod)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil SpectraSyn Ultra™ 1000 High VI Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn Elite™ 300 Metallocene Polyalphaolefin Fluid
ExxonMobil SpectraSyn Ultra™ 300 High VI Polyalphaolefin (PAO) Fluid
ChevronTexaco Cetus® PAO 100
ExxonMobil ACHIEVE 3825 Exxpol Metallocene Grade for Nonwovens Fiber and General Extrusion Applications

PEX99679 / 175915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.