MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Silicon Nitride/Aluminum Nitride/Aluminum Oxide (Sialon)
Categories: Ceramic; Nitride

Material Notes: Sialon® is a solid solution of Silicon Nitride with Aluminum Oxide and Aluminum Nitride. It exhibits high strength at high temperatures, is hard, tough and wear resistant. It is chemically inert and thermal shock resistant. These properties all make Sialon® applied for foundry use, including use as containers for molten metals. Sialon® is non-wetting for most non-ferrous metals up to 1000°C. It has found use as thermocouple sheaths and its high wear resistance lends itself to components such as extrusion tools drawing dies and plugs. Sialon® can be machined as for Tungsten Carbide and the surface finish improved by diamond grinding.

Information provided by Goodfellow.

Key Words: Syalon®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.24 g/cc
Porosity 0.010 %Apparent
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 1650 - 1800kgf/mm²
Tensile Modulus 280 - 300 GPa
Compressive Strength >= 3500 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 - 1.00e+17 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.30 - 3.70 µin/in-°F
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.620 - 0.710 J/g-°C
@Temperature 25.0 °C
Thermal Conductivity 20.0 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 1000 °Ccontinuous
 
Descriptive Properties
Chemical Resistance - AlkalisFair
Chemical Resistance - Concentrated AcidsGood
Chemical Resistance - Dilute AcidsGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Nitride, Sialon
Silicon Nitride, RBSN
Silicon Nitride, reaction sintered
Grade 705 Zirconium (Zr-2.5Nb)
Grade 706 Zirconium (Zr-2.5Nb)

CGOODF249 / 197412

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.